General purpose render/plaster, blend of ordinary portland cement, hydrated lime and properly graded fillers combined with chemical additives as improving agents.·The plaster is specially formulated for one coat application by plastering machine that mix and spry in one operation or by hand.
Additional Info
-
Product Description
- Type: powder
- Grading: 0-1.5mm
- Colour: grey
- Bulk Density: 1.65 Kg/lit
- Inflammability: NO
- Health Hazard: NO
-
Characteristics of Mix
- Mixing ratio (water/dry material): 0.24
- Volume yield of wet mix: 690 lit/ton
- Weight of fresh mortar: 1.45 Kg/lit
- PH of mix: >12
- Water retention of the mix: good 1*
- Pot life: > 4 hours
- Open time after application: 1 -2 hours 2*
- Minimum thickness: 8mm
- Maximum thickness: 20mm
- Cure time: 14 days
-
Final Performance (Typical Value)
- Compressive strength: >2.5 N/mm2
- Flexural strength: > 1 N/mm2
- Tensile adhesion strength: > 0.20 N/mm2
- Water absorption: W1
- Water vapour permeability co-efficient (µ): μ 25 (tab. value)
- Thermal conductivity: P = 50% λ= 0,83 W/mK (tab. values)
- Weight of hardened mortar: 1.51 Kg/lit
- 1*: Depends on the absorption of the background.
- 2*: Depends on the weather conditions and the absorption of the background.
-